產(chǎn)品詳情
牌號(hào) 1.4571普通用途不銹鋼板和鋼帶
X6CrNiMoTi 17-12-2
對(duì)應(yīng)標(biāo)準(zhǔn) NF EN 10088-2-2005
普通用途不銹鋼板和鋼帶的交貨技術(shù)條件
Part2:Technical delivery conditions for sheet/plate and strip of corrosion resisting steels for general purposes
歸類 奧氏體不銹鋼
標(biāo)簽 標(biāo)準(zhǔn)等級(jí)
X6CrNiMoTi17-12-2 化學(xué)元素成分含量(%)
成分 | C | Si | Mn | P | S ① | Cr | Ni | Mo | 更多 |
最小值 | - | - | - | - | - | 16.5 | 10.5 | 2 | Ti:5×C~0.7 |
最DA值 | 0.08 | 1 | 2 | 0.045 | 0.015 | 18.5 | 13.5 | 2.5 |
X6CrNiMoTi17-12-2 機(jī)械性能 | |||||
條件 | 熱處理或狀態(tài) | 抗拉強(qiáng)度 | 屈服點(diǎn) | 斷后伸長(zhǎng)率或延伸率 | 沖擊吸收能量 |
σb | σs | δ | KV2 | ||
Mpa | Mpa | % | J | ||
冷軋帶鋼:T ≤ 8mm | +AT | 540~690 | ( t ) | ( t ) | - |
Rp0.2:≥ 240①③ | T<3mm:≥40③④ | ||||
Rp1.0:≥ 270①② | T ≥ 3mm:≥40③⑤ | ||||
③ | |||||
熱軋帶鋼:T ≤ 13.5mm | +AT | 540~690 | ( t ) | ( t ) | (T>10mm) |
Rp0.2:≥ 220①③ | T<3mm:≥40③④ | I:≥ 100;t:≥60 | |||
Rp1.0:≥ 260①② | T ≥ 3mm:≥40③⑤ | ||||
③ | |||||
熱軋中厚板:T ≤ 75mm⑥ | +AT | 520~670 | ( t ) | ( t ) | (T>10mm) |
Rp0.2:≥ 220①③ | T<3mm:≥40③④ | I:≥ 100;t:≥60 | |||
Rp1.0:≥ 260①② | T ≥ 3mm:≥40③⑤ | ||||
③ | |||||
鋼材(工藝流程2H): | 冷加工+C700⑦⑧ | 700~850 | |||
鋼材(工藝流程2H): | 冷加工+C850⑦⑧ | 850~1000 | |||
鋼材(工藝流程2H): | 冷加工+CP350⑦⑧ | 350~500 | |||
鋼材(工藝流程2H): | 冷加工+CP500⑦⑧ | 500~700 |